/*! This file is auto-generated */ .wp-block-button__link{color:#fff;background-color:#32373c;border-radius:9999px;box-shadow:none;text-decoration:none;padding:calc(.667em + 2px) calc(1.333em + 2px);font-size:1.125em}.wp-block-file__button{background:#32373c;color:#fff;text-decoration:none} Problem 84 Superalloys have been made of ni... [FREE SOLUTION] | 91Ó°ÊÓ

91Ó°ÊÓ

Superalloys have been made of nickel and aluminum. The alloy owes its strength to the formation of an ordered phase, called the gamma-prime phase, in which Al atoms are at the corners of a cubic unit cell and Ni atoms are at the face centers. What is the composition (relative numbers of atoms) for this phase of the nickel-aluminum superalloy?

Short Answer

Expert verified
The composition of the gamma-prime phase in the nickel-aluminum superalloy is 25% Al and 75% Ni, which is derived from one Al atom and three Ni atoms per unit cell.

Step by step solution

01

Find the number of Al atoms

There is one Al atom at each corner of the cubic unit cell. Since a cube has 8 corners, there are a total of 8 Al atoms at the corners.
02

Calculate the fraction of Al atoms at each corner that belong to the unit cell

Each Al atom at a corner of the cube is shared by 8 other unit cells. So, the fraction of each Al atom at a corner that belongs to the unit cell is 1/8.
03

Find the total number of Al atoms per unit cell

Considering the fraction we found in step 2, there are \(8 \times \frac{1}{8} = 1\) Al atom per unit cell.
04

Find the number of Ni atoms

There is one Ni atom at each face center of the cubic unit cell. Since a cube has 6 faces, there are a total of 6 Ni atoms at the face centers.
05

Calculate the fraction of Ni atoms at each face center that belong to the unit cell

Each Ni atom at a face center is shared by 2 unit cells. So, the fraction of each Ni atom at a face center that belongs to the unit cell is 1/2.
06

Find the total number of Ni atoms per unit cell

Considering the fraction we found in step 5, there are \(6 \times \frac{1}{2} = 3\) Ni atoms per unit cell.
07

Calculate the composition of the gamma-prime phase

The composition of the gamma-prime phase is the ratio of the total number of Al atoms to the total number of atoms in the unit cell. The total number of atoms in the unit cell is the sum of the Al atoms and Ni atoms: \(1 + 3 = 4\). Therefore, the composition of the gamma-prime phase is expressed as the ratio of Al atoms to the total number of atoms: \(\frac{1}{4}\) or 25% Al and 75% Ni.

Unlock Step-by-Step Solutions & Ace Your Exams!

  • Full Textbook Solutions

    Get detailed explanations and key concepts

  • Unlimited Al creation

    Al flashcards, explanations, exams and more...

  • Ads-free access

    To over 500 millions flashcards

  • Money-back guarantee

    We refund you if you fail your exam.

Over 30 million students worldwide already upgrade their learning with 91Ó°ÊÓ!

Key Concepts

These are the key concepts you need to understand to accurately answer the question.

Nickel-Aluminum Superalloy
Nickel-aluminum superalloys are a class of materials that are highly sought after for their exceptional mechanical properties, which remain stable even at high temperatures. These superalloys are primarily used in aerospace and power generation industries where components are subjected to extremely harsh conditions, requiring materials that can withstand high stresses, corrosion, and thermal degradation.

The superalloys are composed of a base metal of nickel with aluminum added along with other elements such as titanium and chromium to enhance specific properties. The unique strength of nickel-aluminum superalloys comes from the presence of different phases within the alloy, in particular the gamma-prime (\f\(\text{gamma-prime}\f\)) phase. This phase is essential for the alloy's ability to maintain its strength under high temperatures, a key requirement for parts such as turbine blades and jet engines.

The understanding of the composition and properties of the gamma-prime phase is fundamental not only for material science students but also for engineers involved in designing components that make use of these superalloys. Blending the right amount of nickel and aluminum can create various compositions, which allows engineers to tailor the material properties to suit specific applications.
Cubic Unit Cell
The structure of crystalline solids is often explained in terms of the unit cell, which is the smallest repeating unit of the crystal lattice that exhibits the full symmetry of the crystal structure. In the context of the gamma-prime phase in nickel-aluminum superalloys, the cubic unit cell is of particular interest.

A cubic unit cell has sides of equal length and all angles between its edges are 90 degrees. This symmetry makes it easier to understand and calculate the arrangement of atoms within the cell. There are several types of cubic unit cells, but in the case of the gamma-prime phase, we focus on a face-centered cubic (FCC) structure where atoms are located at each of the corners and the centers of the faces of the cube. This specific arrangement greatly contributes to the distinctive properties of the phase, such as high resistance to creep and prolonged strength at elevated temperatures.

Understanding the geometric configuration of the cubic unit cell and its significance in the properties of materials can enhance a student's grasp of both crystallography and materials science.
Alloy Phase Structure
The alloy phase structure is critical in determining the behavior and properties of an alloy. Different phases have distinct atomic arrangements, which result in varied mechanical properties such as strength, ductility, and resistance to deformation at high temperatures.

In nickel-aluminum superalloys, the alloy phase structure is characterized by the combination of a gamma matrix and the gamma-prime precipitates. The gamma matrix is a solid solution phase that provides ductility, while the gamma-prime phase is an intermetallic compound that confers strength by obstructing dislocation motion. The gamma-prime phase, specifically in nickel-aluminum alloys, has Al atoms at the corners of the cubic unit cell with Ni atoms at the face centers, creating an ordered structure within the FCC matrix.

This intimate mixture of phases is engineered to yield superior mechanical properties and is a prime example of how material scientists use phase diagrams and solid-state chemistry to tailor materials for demanding applications.
Crystal Lattice and Unit Cells
The concept of the crystal lattice connects directly to the understanding of unit cells. A crystal lattice is a three-dimensional arrangement of atoms, ions, or molecules in a crystalline material. This arrangement is orderly and periodic, extending in all spatial directions.

The unit cell is like a building block of the crystal lattice; it is the smallest component that, when stacked together with identical cells in three-dimensional space, will replicate the entire crystal structure. This is akin to using a single type of block to build a large structure - the pattern repeats, leading to the macroscopic crystal. By analyzing the unit cell, scientists gain insights into the properties and behavior of the entire crystal structure.

For students, understanding the relationship between crystal lattice and unit cells is pivotal for grasping how different materials are formed and how their structure affects their properties. In the specific context of nickel-aluminum superalloys, knowing that the gamma-prime phase is structured in an FCC unit cell helps explain why these materials can handle high-temperature applications, making this knowledge not only academic but also highly practical.

One App. One Place for Learning.

All the tools & learning materials you need for study success - in one app.

Get started for free

Most popular questions from this chapter

When 1 mole of benzene is vaporized at a constant pressure of 1.00 atm and at its boiling point of \(353.0 \mathrm{K}, 30.79 \mathrm{kJ}\) of energy (heat) is absorbed and the volume change is +28.90 L. What are \(\Delta E\) and \(\Delta H\) for this process?

A common prank on college campuses is to switch the salt and sugar on dining hall tables, which is usually easy because the substances look so much alike. Yet, despite the similarity in their appearance, these two substances differ greatly in their properties, since one is a molecular solid and the other is an ionic solid. How do the properties differ and why?

X rays from a copper X-ray tube \((\lambda=154 \mathrm{pm})\) were diffracted at an angle of 14.22 degrees by a crystal of silicon. Assuming first-order diffraction \((n=1\) in the Bragg equation), what is the interplanar spacing in silicon?

A 0.132 -mole sample of an unknown semiconducting material with the formula XY has a mass of \(19.0 \mathrm{g}\). The element X has an electron configuration of \([\mathrm{Kr}] 5 s^{2} 4 d^{10} .\) What is this semiconducting material? A small amount of the Y atoms in the semiconductor is replaced with an equivalent amount of atoms with an electron configuration of \([\mathrm{Ar}] 4 s^{2} 3 d^{10} 4 p^{5} .\) Does this correspond to n-type or p-type doping?

Pyrolusite is a mineral containing manganese ions and oxide ions. Its structure can best be described as a body-centered cubic array of manganese ions with two oxide ions inside the unit cell and two oxide ions each on two faces of the cubic unit cell. What is the charge on the manganese ions in pyrolusite?

See all solutions

Recommended explanations on Chemistry Textbooks

View all explanations

What do you think about this solution?

We value your feedback to improve our textbook solutions.

Study anywhere. Anytime. Across all devices.